Solving Chalk Run Down ProblemsSupport2021-05-17T09:34:52-04:00
CHALK RUN-DOWN
The washing down of chalk from an excessively eroding paint onto another area below (a brick foundation, for example), ruining its appearance (see Chalking).
POSSIBLE CAUSES:
- Use of a lower quality, highly pigmented paint.
- Use of an interior paint for an outdoor application.
- Erosion of factory-finished metal siding.
SOLUTION:
- Remove as much of the chalk residue as possible (see Chalking). Scrub any stained areas with a stiff brush, using a detergent solution; rinse thoroughly. In cases of severe staining, an acid wash may be necessary. Either way, if the affected area dries to a different color, consider painting it with a quality latex paint. Eroding aluminum siding should be thoroughly cleaned (power washing recommended) before painting with a quality exterior latex paint.
Note: Images & information provided by The Rohm & Hass Paint Quality Institute.